Umgangatho ophezulu weFayibha yeglasi eThungelweyo idityaniswe neFiberglass Mat eLongitudinal Triaxial Fabric yokulungisa iBlade
Ineentlobo ezimbini njengoko kungezantsi:
I-Longitudinal Triaxial 0º/+45º/-45º
Transverse Triaxial +45º/90º/-45º
Ifoto:
Iimpawu zeMveliso:
- Akukho binder, ifanelekile kwiinkqubo ezahlukeneyo ze-resin
- Ineempawu ezilungileyo zoomatshini
- Inkqubo yokusebenza ilula kwaye ixabiso liphantsi
Usetyenziso:
I-Triaxial combo mat isetyenziswa kwiincakuba zeeinjini zomoya, ukwenziwa kweenqanawa kunye neengcebiso zemidlalo.Ilungele zonke iintlobo zeenkqubo zokuqinisa i-resin, njenge-resin ye-polyester engaxutywanga, i-vinyl resin kunye ne-epoxy resin.
Uluhlu lweeMveliso
Inombolo yeMveliso | Uxinaniso lulonke | 0 ° ukuxinana okujikelezayo | +45 ° ukuxinana okujikelezayo | -45 ° ukuxinana okujikelezayo |
| (g/m2) | (g/m2) | (g/m2) | (g/m2) |
BH-TLX600 | 614.9 | 3.6 | 300.65 | 300.65 |
BH-TLX750 | 742.67 | 236.22 | 250.55 | 250.55 |
BH-TLX1180 | 1172.42 | 661.42 | 250.5 | 250.5 |
BH-TLX1850 | 1856.86 | 944.88 | 450.99 | 450.99 |
BH-TLX1260/100 | 1367.03 | 59.06 | 601.31 | 601.31 |
BH-TLX1800/225 | 2039.04 | 574.8 | 614.12 | 614.12 |
Inombolo yeMveliso | Uxinaniso lulonke | +45 ° ukuxinana okujikelezayo | 90 ° ukuxinana okujikelezayo | -45 ° ukuxinana okujikelezayo | Chop ubuninzi | Ukuxinana komsonto wePolyester |
| (g/m2) | (g/m2) | (g/m2) | (g/m2) | (g/m2) | (g/m2) |
BH-TTX700 | 707.23 | 250.55 | 200.78 | 250.55 |
| 5.35 |
BH-TTX800 | 813.01 | 400.88 | 5.9 | 400.88 |
| 5.35 |
BH-TTX1200 | 1212.23 | 400.88 | 405.12 | 400.88 |
| 5.35 |
BH-TTXM1460/101 | 1566.38 | 424.26 | 607.95 | 424.26 | 101.56 | 8.35 |
Ububanzi obuqhelekileyo kwi-1250mm, 1270mm, kunye nobunye ububanzi bunokwenziwa ngokwesicelo somthengi, obukhoyo ukusuka kwi-200mm ukuya kwi-2540mm.
Ukupakisha& Ugcino:
Ngokuqhelekileyo igqitywe kwi-tube yephepha ene-diameter yangaphakathi ye-76mm, emva koko i-warped roll
ngefilimu yeplastiki kwaye ifakwe kwibhokisi yokuthumela ngaphandle, umthwalo wokugqibela kwiipalethi kunye nobuninzi kwisikhongozeli.
Imveliso kufuneka igcinwe kwindawo epholileyo, engenamanzi.Kucetyiswa ukuba ubushushu begumbi kunye nokufuma kuhlale kugcinwe ku-15℃ ukuya kuma-35℃ kunye nama-35% ukuya kuma-65% ngokulandelelanayo.Nceda ugcine imveliso kwipakethe yayo yokuqala ngaphambi kokuba isetyenziswe, ukuthintela ukufunxa ukufuma.